Method of friction welding

US7997473B2 · kind B2 · utility

1Cited by
14References
29Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 13, 2010
Grant dateAug 16, 2011
Priority date
Expiry dateJul 13, 2030

Classification

  • Technology area (CPC F)Mechanical Engineering; Lighting; Heating
  • CPC primaryF05B2230/239
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

A method of friction welding comprising providing a first workpiece (24) having a first weld surface (38) and a second workpiece (26) having a second weld surface (40). In a first region (42) adjacent the first weld surface (38) the first workpiece (24) is arranged at an angle (α) of substantially 90° to the first weld surface (38) and in a second region (44) adjacent to the first region (42) the first workpiece (24) tapers away from the first weld surface (38). The first workpiece (24) is arranged such that in the second region (44) the first workpiece (24) is arranged at an angle (β) greater than 90° and less than 180° to the first weld surface (38). The first and second workpieces (24, 26) are arranged such that first weld surface (38) of the first workpiece (24) abuts the second weld surface (40) of the second workpiece (26). The first and second workpieces (24, 26) are moved relative to each other such that the temperature increases at the weld surfaces (38, 40) to create a weld interface (46) and then the movement is stopped to cool to weld the first and second workpieces (24, 26) together.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.