Patent · US Active

Method to fabricate inhomogeneous particles

US8007829B2 · kind B2 · utility

1Cited by
2References
32Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 19, 2006
Grant dateAug 30, 2011
Priority date
Expiry dateJul 2, 2030

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2998
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A method for making inhomogeneous microparticles comprises a) providing an amount of each of at least two polyelectrolytes having a charge, b) providing an amount of a counterion having a valence of at least 2, c) combining the polyelectrolytes and the counterion in a solution such that the polyelectrolyte self-assembles to form inhomogeneous aggregates, and d) adding nanoparticles to the solution such that nanoparticles arrange themselves around the inhomogeneous aggregates to form inhomogeneous particles. The polyelectrolyte may have a positive or negative charge. The charge ratio R of total charge of the counterions to the total charge of the polyelectrolyte may be greater than 1.0.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.