Soft magnetic iron/cobalt/chromium-based alloy and process for manufacturing it
US8012270B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 24, 2008 |
| Grant date | Sep 6, 2011 |
| Priority date | — |
| Expiry date | Sep 4, 2029 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01F41/0246
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A soft magnetic alloy consists essentially of 5 percent by weight≦Co≦30 percent by weight, 1 percent by weight≦Cr≦20 percent by weight, 0.1 percent by weight≦Al≦2 percent by weight, 0 percent by weight≦Si≦1.5 percent by weight, 0.017 percent by weight≦Mn≦0.2 percent by weight, 0.01 percent by weight≦S≦0.05 percent by weight where Mn/S is >1.7, 0 percent by weight≦O≦0.0015 percent by weight, und 0.0003 percent by weight≦Ce≦0.05 percent by weight, 0 percent by weight≦Ca≦0.005 percent by weight and the remainder iron, where 0.117 percent by weight≦(Al+Si+Mn+V+Mo+W+Nb+Ti+Ni)≦5 percent by weight.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.