Patent · US Active

Method for making mesoporous material

US8012450B2 · kind B2 · utility

0Cited by
1References
18Claims
0Family size

Assignees

Inventors

Key dates

Filing dateDec 14, 2007
Grant dateSep 6, 2011
Priority date
Expiry dateJun 6, 2030

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2111/94
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for making the mesoporous material includes the following steps: dissolving a nanocrystal powder in an organic solvent, and achieving a solution A with concentration of 1-30 mg/ml; dissolving a surfactant in water, and achieving a solution B with an approximate concentration of 0.002-0.05 mol/ml; mixing the solution A and the solution B in a volume ratio of 1:(5-30), and achieving a mixture; stirring and emulsifying the mixture, until an emulsion C is achieved; removing the organic solvent from the emulsion C, and achieving a deposit; washing the deposit with deionized water, and achieving a colloid; and drying and calcining the colloid, and eventually achieving a mesoporous material. The mesoporous material has a large specific surface area, a high porosity, and a narrow diameter distribution.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.