Method for the production of a foamed slag in a metal bath
US8043402B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 15, 2007 |
| Grant date | Oct 25, 2011 |
| Priority date | — |
| Expiry date | Jan 15, 2027 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/20
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for producing a foamed slag (1) on a metal bath (2) in a metallurgical furnace (3), in which a mixture (4) containing at least one metal oxide and carbon is introduced into the furnace (3), the metal oxide is reduced by the carbon below the slag (1) that is located there, and the gases produced during the reduction process form bubbles such that the slag is foamed. In order to optimize the formation of foamed slag, the mixture (4) is delivered into the furnace (3) in such a way that a desired height (h) or a desired section of the height (h) of the layer of foamed slag (1) is generated or maintained.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.