Patent · US Active

Polyamide molding compound and its use for producing transparent, hot-steam-sterilizable molded parts and extrudates

US8044171B2 · kind B2 · utility

4Cited by
3References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 31, 2006
Grant dateOct 25, 2011
Priority date
Expiry dateJan 18, 2027

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L2205/02
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The invention relates to a polyamide molding material or copolyamide molding material and the use of such a polyamide molding material or copolyamide molding material for producing steam-sterilizable transparent moldings and extrudates. This polyamide molding material is characterized in that it comprises at least one copolyamide formed from 35-42 mol % of bis(4-amino-3-methylcyclohexyl)methane (MACM), 35-42 mol % of isophthalic acid (IPS) and 16-30 mol % of laurolactam (LC12). MACM may be replaced up to 50% by bis(4-aminocyclohexyl)-methane (PACM) and IPA up to 50% by terephthalic acid (TPA). The polyamide molding material may also be a blend of copolyamides or a blend of copolyamides with polyamide 12. The relative viscosity (RV) of the polyamide molding material or copolyamide molding material is in any case adjusted to a value which is greater than 1.45. Steam-sterilizable and transparent standard specimens which are produced from such polyamide molding materials or copolyamide molding materials and whose composition corresponds to the transparent moldings and extrudates have a tensile strain at break which, after undergoing at least 140 and especially preferably at least 350 s…