Method of mitigating against thermal contraction induced cracking during casting of a super Ni alloy

US8056608B2 · kind B2 · utility

1Cited by
14References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 24, 2009
Grant dateNov 15, 2011
Priority date
Expiry dateApr 24, 2029

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22D27/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of mitigating against thermal contraction induced cracking during casting of a super Ni alloy, the method comprising: pouring liquid alloy into a mould such that liquid alloy is present in a feeder of said mould; and inducing an electrical current in alloy in said feeder to reduce a rate of cooling of alloy in said feeder.