High-density pressurelessly sintered zirconium diboride/silicon carbide composite bodies and a method for producing the same

US8097548B2 · kind B2 · utility

1Cited by
26References
5Claims
0Family size

Inventors

Key dates

Filing dateAug 29, 2008
Grant dateJan 17, 2012
Priority date
Expiry dateOct 11, 2028

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2235/963
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of sintering a ZrB2—SiC composite body at ambient pressures, including blending a first predetermined amount of ZrB2 powder with a second predetermined amount of SiC powder, wherein both powders are characterized by the presence of surface oxide impurities. Next the blended powders are mixed to yield a substantially homogeneous powder mixture and a portion of the substantially homogeneous powder mixture is formed into a green body. The body is fired to a first temperature, wherein substantially all surface oxide impurities are reduced and/or volatilized to substantially eliminate oxides from the green body, and the body is heated to a second temperature and sintered to yield a composite body of at least about 99 percent theoretical density (more typically at least about 99.5 percent theoretical density) and characterized by SiC whisker-like inclusions distributed substantially evenly in a ZrB2 matrix.