Patent · US Active

Free cutting steel

US8124008B2 · kind B2 · utility

1Cited by
1References
4Claims
0Family size

Assignees

Inventors

Key dates

Filing dateNov 29, 2002
Grant dateFeb 28, 2012
Priority date
Expiry dateAug 28, 2027

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/60
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A low carbon free cutting steel can be obtained by allowing the steel to contain 0.02 to 0.15 mass % of C, 0.05 to 1.8 mass % of Mn, 0.20 to 0.49 mass % of S, more than 0.01 mass % and not more than 0.03 mass % of O, 0.3 to 2.3% of Cr, and the balance consisting of Fe and inevitable impurities, the Cr/S ratio falling within a range of between 2 and 6.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.