Patent · US Active

Polypropylene composition for air quenched blown films

US8133963B2 · kind B2 · utility

2Cited by
22References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 29, 2009
Grant dateMar 13, 2012
Priority date
Expiry dateMay 26, 2030

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/31938
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The invention is directed to a polypropylene resin, which is suitable for manufacturing an air quenched blown film. The resin has a melt flow rate of greater than 5 g/10 min, less than 2% xylene solubles, a pentad isotacticity of greater than 95%, an isotactic pentad/triad ratio of greater than 95%, a crystallinity of at least 65%, and a crystallization temperature of at least 127° C. The polypropylene resin contains from 500 ppm to 2500 ppm of a nucleator/clarifier additive. An quenched blown film made from resin exhibits a crystallization onset temperature of at least 116° C. and a crystallization half-life time of less 4.1 seconds or less when tested using fast DSC analysis with a scan rate of 200° C./minute.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.