Patent · US Active

Method of production of steel superior in machinability

US8137484B2 · kind B2 · utility

1Cited by
5References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 20, 2008
Grant dateMar 20, 2012
Priority date
Expiry dateApr 6, 2029

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/009
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention provides steel superior in machinability comprised of, by wt %, C: 0.005 to 0.2%, Si: 0.001 to 0.5%, Mn: 0.2 to 3.0%, P: 0.001 to 0.2%, S: 0.03 to 1.0%, T.N: 0.002 to 0.02%, T.O: 0.0005 to 0.035%, and the balance of Fe and unavoidable impurities, said steel satisfying one or both of Mn/S in the steel being 1.2 to 2.8 or an area ratio of pearlite over a grain size of 1 μm in a microstructure of the steel being not more than 5%.