The invention relates to a wood-based lignocellulosic fibrous material having a tearing length of more than 8 km at 15° SR and a lignin content of at least 15%, based on the unbleached oven-dry fibrous material, for coniferous wood and having a tearing length of more than 5.0 km at 20° SR and a lignin content of at least 12%, based on the unbleached oven-dry fibrous material, for deciduous wood.