Patent · US Active

Austenitic stainless steel, manufacturing method for the same, and structure using the same

US8172959B2 · kind B2 · utility

2Cited by
6References
11Claims
0Family size

Assignees

Inventors

Key dates

Filing dateJan 13, 2005
Grant dateMay 8, 2012
Priority date
Expiry dateDec 11, 2026

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/13
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

There are provided an austenitic stainless steel having high stress corrosion crack resistance, characterized by containing, in percent by weight, 0.030% or less C, 0.1% or less Si, 2.0% or less Mn, 0.03% or less P, 0.002% or less S, 11 to 26% Ni, 17 to 30% Cr, 3% or less Mo, and 0.01% or less N, the balance substantially being Fe and unavoidable impurities; a manufacturing method for an austenitic stainless steel, characterized in that a billet consisting of the said austenitic stainless steel is subjected to solution heat treatment at a temperature of 1000 to 1150° C.; and a pipe and a in-furnace structure for a nuclear reactor to which the said austenitic stainless steel is applied.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.