Crosslinkable elastomer composition and molded article using the same
US8173727B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Nov 3, 2008 |
| Grant date | May 8, 2012 |
| Priority date | — |
| Expiry date | Jan 17, 2031 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L101/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present invention provides a crosslinkable elastomer composition, in which generation of HF under high temperature conditions is reduced, the decrease in weight to both NF3 plasma treatment and O3 treatment in the semiconductor manufacturing process is small and generation of foreign substances (particles) in these treatments is suppressed significantly. Specifically, the present invention relates to a crosslinkable elastomer composition comprising a crosslinkable elastomer and a filler having a specific surface area of at least 0.5 m2/g and containing a synthetic polymer having a thermally and chemically stable aromatic ring in the main chain, a crosslinkable elastomer composition comprising a crosslinkable elastomer and nonoxide ceramics and a crosslinkable elastomer composition wherein the decrease in weight by NF3 plasma irradiation is at most 0.20%.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.