Slurry phase polymerisation process

US8183334B2 · kind B2 · utility

0Cited by
0References
38Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 29, 2008
Grant dateMay 22, 2012
Priority date
Expiry dateFeb 1, 2029

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08F110/02
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80 wt % of a low molecular weight (LMW) polymer is made in suspension in a second reactor in the presence of the HMW polymer, wherein the solids concentration in the second LMW reactor, defined as the mass of polymer divided by the total mass of slurry, is at least 35 wt %, most preferably between 45 wt % and 60 wt %, and/or the ratio of solids concentration in the first reactor to that in the second reactor is maintained at less than 1.0, preferably between 0.6 and 0.8, and further wherein the volume of the second reactor is at least 10%, preferably at least 30% and more preferably at least 50% greater than the volume of the first reactor.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.