Water/oil repellent composition, method for its production and method for treating article
US8193277B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 21, 2011 |
| Grant date | Jun 5, 2012 |
| Priority date | — |
| Expiry date | Oct 21, 2031 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F220/20
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
To provide a water/oil repellent composition which is capable of imparting sufficient dynamic water repellency and post-air-drying water repellency to the surface of an article and which presents a low environmental impact, a method for its production and a method for treating an article.A water/oil repellent composition which comprises a copolymer having structural units based on the following monomer (a) and structural units based on the following monomer (b) and having a mass average molecular weight of at least 40,000, and a medium, is used. Monomer (a): a compound represented by (Z—Y)nX, wherein Z is a C1-6 polyfluoroalkyl group or the like, Y is a bivalent organic group or the like, n is 1 or 2, and X is a polymerizable unsaturated group. Monomer (b): an olefin, a homopolymer of which has a glass transition temperature of from −50° C. to 50° C.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.