Patent · US Active

Natural tourmaline anion fiber and filter and producing method

US8231968B2 · kind B2 · utility

5Cited by
10References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 3, 2006
Grant dateJul 31, 2012
Priority date
Expiry dateJun 25, 2028

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2969
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

The present invention provides to a method of producing fiber from tourmaline anion fiber; of which, polypropylene or polyethylene chip, TPE and submicrometer tourmaline particle are prepared and then rolled into submicrometer tourmaline agglomerate through granulation by double screw; then, take submicrometer tourmaline agglomerate and polypropylene or polyethylene chip, of which the content of tourmaline agglomerate accounts for 1˜10% of gross weight, and TPE for 1˜40% of gross weight; tourmaline agglomerate and polypropylene or polyethylene are melted into composite fiber or filter material via spinning, such that the fiber or filter material can yield anion and present outstanding gas permeability and mechanical property.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.