Patent · US Active

Cordierite-based sintered body

US8242039B2 · kind B2 · utility

5Cited by
3References
17Claims
0Family size

Assignee

Inventor

Key dates

Filing dateOct 22, 2010
Grant dateAug 14, 2012
Priority date
Expiry dateDec 5, 2030

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2235/963
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention is intended to drastically improve a precision polishing characteristic of a cordierite-based sintered body which has low thermal expansibility, high dimensional long-term stability and high rigidity (high elastic modulus). The cordierite-based sintered body comprises cordierite as primary components, and one or more selected from the group consisting of La, Ce, Sm, Gd, Dy, Er, Yb and Y in an oxide-equivalent amount of 1 to 8 mass %, without any crystal phase other than a cordierite crystal phase. A mass ratio of primary components of the cordierite satisfies the following relations: 3.85≦SiO2/MgO≦4.60, and 2.50≦Al2O3/MgO≦2.70, and the cordierite-based sintered body after being subjected to precision polishing has a precisely polished surface with an average surface roughness (Ra) of 1 nm or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.