Patent · US Active

Concrete with a low clinker content

US8246739B2 · kind B2 · utility

9Cited by
5References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 24, 2008
Grant dateAug 21, 2012
Priority date
Expiry dateMar 16, 2029

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02W30/91
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A process for the preparation of a wet concrete composition, including mixing Portland clinker in the form of grains having a Dv97 from 10 to 30 μm or having a Blaine specific surface greater than or equal to 5300 cm2/g; slag; calcium sulphate; complementary materials, having a Dv90 less than or equal to 200 μm; from 1500 to 2200 kg/m3 of aggregates; a plasticizer; optionally an accelerator and/or an air-entraining agent and/or a thickening agent and/or a retarder and/or a clay-inerting agent; with 140 to 220 l/m3 of effective water, the total quantity of clinker in the wet concrete being less than or equal to 200 kg/m3.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.