Elastomeric polymer blends and processes for their production
US8247495B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 27, 2011 |
| Grant date | Aug 21, 2012 |
| Priority date | — |
| Expiry date | Jan 27, 2031 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2314/06
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Elastomeric polymer blends and processes for their production are described. Specifically, the polymer blends comprise a first polymer and a second polymer, where the first polymer comprises from about 70 wt % to about 90 wt % units derived from propylene and from about 10 wt % to about 30 wt % units derived from ethylene and/or a C4-C10 alpha-olefin, and the second polymer comprises from about 88 wt % to about 98 wt % units derived from propylene and from about 2 wt % to about 12 wt % units derived from ethylene and/or a C4-C10 alpha-olefin. The elastomeric polymer blends are further characterized by having two or more of the following properties: an overall propylene content of between about 75 wt % and about 90 wt %, a melting point between about 110° C. and about 145° C., a Vicat softening point greater than about 45° C., a tensile stress at 300% strain of less than about 500 psi (3447 kPa), as determined by a stress strain test according to ASTM D412, or an average maximum force for pellet separation of less than about 10 N in an accelerated storage stability test. The polymer blends are produced in a dual reactor process, in which the first polymer and the second polymer are …
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.