Method of extracting Te and bismuth oxide and recovering byproducts

US8277772B2 · kind B2 · utility

0Cited by
2References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 2, 2009
Grant dateOct 2, 2012
Priority date
Expiry dateSep 22, 2029

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P10/20
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of extracting Te and bismuth oxide and recovering byproduct comprises: leaching raw materials with a Te content of ≧1.8% by utilizing a leaching system containing H2SO4, Cl−, Br−, NH4+ and NaClO3, reducing leach solution with SO2 gas by precipitation method after separating impurities from it, washing with concentrated hydrochloric acid to obtain tellurium precipitation (18), purifying to obtain Te with a purity of higher than 99.99%. The filtrate produced is used for extracting Bi2O3 with a purity of higher than 99.99% when Bi content in the raw material is ≧2%. Acidic waste solution produced during the process could be returned to the leaching step for recycle.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.