Patent · US Active

NiMnZn based ferrite

US8282853B2 · kind B2 · utility

21Cited by
4References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 22, 2009
Grant dateOct 9, 2012
Priority date
Expiry dateApr 7, 2031

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01F41/0246
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A novel NiMnZn-based ferrite which can reduce magnetic loss (core loss) at a high frequency of about 2 MHz or higher and achieve higher saturated magnetic flux density while forming high sintered density is provided. The NiMnZn-based ferrite contains a main component comprising 54.0 to 57.5 mol % of iron oxide in terms of Fe2O3, 2.0 to 7.0 mol % of zinc oxide in terms of ZnO, 0.5 to 4.7 mol % of nickel oxide in terms of NiO, and a remainder of manganese oxide (in terms of MnO); and an accessory component comprising 100 to 1000 ppm by weight of Si in terms of SiO2, 800 to 3000 ppm by weight of Ca in terms of CaCO3, and 520 to 1000 ppm by weight of Nb in terms of Nb2O5 with respect to the main component; while having an average ferrite crystal particle size of 2.1 to 8.5 μm.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.