Low energy milling method, low crystallinity alloy, and negative electrode composition
US8287772B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 14, 2009 |
| Grant date | Oct 16, 2012 |
| Priority date | — |
| Expiry date | Jul 28, 2030 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A method of making nanostructured alloy particles includes milling a millbase in a pebble mill containing milling media. The millbase comprises: (i) silicon, and (ii) at least one of carbon or a transition metal, and wherein the nanostructured alloy particles are substantially free of crystalline domains greater than 50 nanometers in size. A method of making a negative electrode composition for a lithium ion battery including the nanostructured alloy particles is also disclosed.