Patent · US Active

Method for preparing cathode active material of lithium battery

US8303841B2 · kind B2 · utility

20Cited by
5References
16Claims
0Family size

Assignees

Inventors

Key dates

Filing dateSep 10, 2010
Grant dateNov 6, 2012
Priority date
Expiry dateMar 24, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A method for preparing a cathode active material of lithium battery is shown. The method includes providing MnOOH and lithium source material, and mixing the MnOOH and the lithium source material in a liquid solvent to achieve a mixture. Then, the mixture is dried to remove the liquid solvent, thereby achieving a precursor. A temperature of the precursor is elevated from room temperature to a sintering temperature of about 500° C. to about 900° C. at a uniform rate, and the precursor is sintered at the sintering temperature for about 3 hours to about 24 hours.