Method for producing a photovoltaic module
US8313973B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 11, 2011 |
| Grant date | Nov 20, 2012 |
| Priority date | — |
| Expiry date | Mar 17, 2031 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E10/50
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A method for producing a photovoltaic module by contacting at least one layer of liquid encapsulant and a plurality of solar cells. The liquid encapsulant has two components. The first component is an acrylic polyol having a terminal hydroxy group, an average number of hydroxy-functional monomer units per polymer chain from 2 to 25 and Mn from 1,000 to 10,000. The second component is an aliphatic polyisocyanate with an average functionality of at least two. The molar ratio of non-terminal hydroxy groups in the polyol to isocyanate groups in the aliphatic polyisocyanate is from 0.5:1 to 1:0.5.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.