Patent · US Active

Dielectric ceramic composition and ceramic electronic component

US8335073B2 · kind B2 · utility

4Cited by
7References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 9, 2011
Grant dateDec 18, 2012
Priority date
Expiry dateJul 26, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2235/79
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A dielectric ceramic composition includes, as a main component, a compound having perovskite type crystal structure shown by a general formula ABO3, as subcomponents, in terms of respective element with respect to 100 moles of the compound, and 0.6 to 2.0 moles of an oxide of Mg, 0.010 to 0.6 mole of oxide of Mn and/or Cr, 0.010 to 0.2 mole of an oxide of at least one selected from V, Mo and W, 0.10 to 1.0 mole of an oxide of R1 (R1 is at least one selected from Y, Yb, Er and Ho), 0.10 to 1.0 mole of an oxide of R2 (R2 is at least one selected from Dy, Gd and Tb) and 0.2 to 1.5 moles of a component consisting of an oxide of Ba and/or oxide of Ca and an oxide of Si. According to the present invention, even when a dielectric layer is made thinner, a dielectric ceramic composition having good characteristics can be provided.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.