Implantable material and a method for the preparation thereof
US8337938B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Feb 8, 2012 |
| Grant date | Dec 25, 2012 |
| Priority date | — |
| Expiry date | Feb 8, 2032 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L89/00
- WIPO fieldMedical technology
- WIPO sectorInstruments
Abstract
A method for the preparation of a regenerated silk fibroin solution comprises the steps of: treating silk or silk cocoons with an ionic reagent comprising an aqueous solution of monovalent cations and monovalent anions, the cations and anions having ionic radii of at least 1.05 Angstroms and a Jones-Dole B coefficient of between −0.001 and −0.05 at 25° C.; and subsequently degumming the treated silk or silk cocoons; or alternatively, degumming silk or silk cocoons; and subsequently treating the degummed silk or silk cocoons with an ionic reagent comprising an aqueous solution of monovalent cations and monovalent anions, the cations and anions having ionic radii of at least 1.05 Angstroms and a Jones-Dole B coefficient of between −0.001 and −0.05 at 25° C. The invention also extends to fibroin solution, a fibroin material and an implant useful for cartilage repair.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.