Patent · US Active

High tensile strength steel having favorable delayed fracture resistance and method for manufacturing the same

US8357252B2 · kind B2 · utility

0Cited by
1References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 31, 2008
Grant dateJan 22, 2013
Priority date
Expiry dateJul 3, 2028

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/06
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

High tensile strength steels that have both favorable delayed fracture resistance and a tensile strength of 600 MPa or higher and are suitably used in construction machinery, tanks, penstocks, and pipelines, as well as methods for manufacturing such steels are provided. The safety index of delayed fracture resistance (%) is 100×(X1/X0), where X0: reduction of area of a specimen substantially free from diffusible hydrogen, and X1: reduction of area of a specimen containing diffusible hydrogen.