Abstract
The present invention relates to a process for obtaining neopentyl glycol by hydrogenating cracking of high-boilers occurring in the production process in the presence of copper-chromite catalysts. The hydrogenating cracking proceeds in the absence of solvent at a temperature of 140 to 220° C. and at pressures of 7 to 28 MPa.