Abstract
The alkaline earth metal aluminosilicate glass for light bulbs with molybdenum parts has a composition (in percent by weight on an oxide basis) of SiO2, 56-60; Al2O3, 17-18; B2O3, 0.5-2; MgO, 0.5-2; CaO, >14-15.5; SrO, 0-3; BaO, 6-8; ZrO2, 0-5; CeO2, 0-0.1 and TiO2, 0-0.5.