High post consumer content mineral filler based on micronized recycled asphalt paving and thermoplastic compositions and polymeric emulsions derived from same

US8367759B2 · kind B2 · utility

0Cited by
6References
17Claims
0Family size

Inventors

Key dates

Filing dateFeb 11, 2011
Grant dateFeb 5, 2013
Priority date
Expiry dateFeb 11, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02W30/91
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A micronized filler for use in thermoplastic compositions, polymeric emulsions and other end products can include micronized recycled asphalt paving. The recycled asphalt paving filler can include calcium carbonate, calcium magnesium carbonate and silicon dioxide. The filler can have a particle size of 325 mesh screen, and a specific gravity of 2.4. The filler increases the post consumer content of various end products.