Biaxially oriented polypropylene film
US8378047B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 9, 2009 |
| Grant date | Feb 19, 2013 |
| Priority date | — |
| Expiry date | Jan 9, 2029 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08J2323/12
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present technology relates to a biaxially oriented polypropylene film. The biaxially oriented polypropylene film comprises a polypropylene material having xylene solubles of at least 0.5 percent by weight. The polypropylene also has a strain hardening index of at least 0.15 measured at a deformation rate dε/dt of 1.00 s−1 at a temperature of 180° C. In certain embodiments, the strain hardening index is defined as the slope of a logarithm to the basis 10 of a tensile stress growth function as a function of a logarithm to the basis 10 of a Hencky strain for the range of Hencky strains between 1 and 3.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.