Patent · US Active

Utilization of moisture in hermetically sealed solid electrolytic capacitor and capacitors made thereof

US8379371B2 · kind B2 · utility

4Cited by
11References
40Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 20, 2011
Grant dateFeb 19, 2013
Priority date
Expiry dateSep 30, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/435
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A method for forming a hermetically sealed capacitor including: forming an anode; forming a dielectric on the anode; forming a conductive layer on the dielectric thereby forming a capacitive element; inserting the capacitive element into a casing; electrically connecting the anode to an exterior anode connection; electrically connecting the cathode to an exterior cathode connection; filling the casing with an atmosphere comprising a composition, based on 1 kg of atmosphere, of at least 175 g to no more than 245 g of oxygen, at least 7 g to no more than 11 g of water, at least 734 grams to no more than 818 grams of nitrogen and no more than 10 grams of a minor component; and hermetically sealing the casing with the atmosphere with the capacitive element contained in the casing.