Patent · US Active

Single-phase hydraulic binder, methods for the production thereof and building material produced therewith

US8382892B2 · kind B2 · utility

8Cited by
4References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 16, 2008
Grant dateFeb 26, 2013
Priority date
Expiry dateJun 12, 2029

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P40/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The invention relates to a monophase amorphous hydraulic binder containing silicon, calcium and oxygen atoms in an arrangement comprising silicate building units having an average connectedness of at least Q1, with none or a part of the calcium atoms being substituted for by a metal atom M[6]x+ sixfold or higher-coordinated with oxygen and/or none or no more than 45 atomic percent of the silicon atoms being substituted for by a metal atom M[4]y+ tetrahedrally coordinated with oxygen, the molar ratio of[CaO+(x/2)·(M[6]x+Ox/2)]:[SiO2+M[4]y+Oy/2]having a value of 0.2 to 1.5, and the binder having less than 3.5% by weight of water, as well as a mixture containing this binder.Furthermore, the invention relates to methods for manufacturing the binder or a mixture containing this binder by reaction grinding a starting material containing silicate building units having a connectedness of Q0 to Q2, with a solid silicate raw material having a connectedness of the silicate building units of Q3 to Q4 and optionally drying the monophase hydraulic binder to a water content of below 3.5% by weight.Finally, the invention relates to a building material made by setting the binder or a mixture contai…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.