Process for manufacturing mineral wool, cobalt-based alloys for the process and other uses

US8398791B2 · kind B2 · utility

0Cited by
7References
12Claims
0Family size

Assignees

Inventors

Key dates

Filing dateAug 23, 2007
Grant dateMar 19, 2013
Priority date
Expiry dateSep 3, 2028

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C19/07
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Cobalt based alloys exhibiting high-temperature mechanical strength in an oxidizing medium are provided. The alloys are free of W and Hf and include the following elements in percentage by weight of the alloy: 23 to 34% Cr; 6 to 12% Ni; 6.0 to 10% Ta; 0.3 to 1.2% C; less than 3% Fe; less than 1% Si; less than 0.5% Mn; less than 0.1% Zr; and a balance of cobalt and impurities. Ta/C molar ratios of the alloys are at least 0.3.