Green joining ceramics

US8398796B2 · kind B2 · utility

1Cited by
8References
32Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 20, 2007
Grant dateMar 19, 2013
Priority date
Expiry dateNov 10, 2030

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T156/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A method of green joining ceramic components is disclosed, particularly for use in forming a discharge body for a ceramic metal halide lamp. The process includes providing a first green ceramic component having a male joining surface, and providing a second green ceramic component having a female joining surface dimensioned to matingly receive the first component. The first and second green ceramic components are assembled along the joining surfaces, the assembled components are uniformly heated to join the first and second components. The joined components are next cooled in a cooling bath that uniformly cools the joined components. Thereafter, the joined green part may be inserted in the furnace for debindering and sintering.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.