Curable compound comprising silylated polyurethane
US8431675B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jun 2, 2010 |
| Grant date | Apr 30, 2013 |
| Priority date | — |
| Expiry date | Mar 9, 2031 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08G2190/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A method for producing a silylated polyurethane including the steps: (A) converting (i) at least polyol compound having a molecular weight of 4,000-30,000 g/mol and at least one monofunctional compound relative to isocyanates and (ii) at least one diisocyanate at a stoichiometric excess of the sum of the polyol compound(s) and monofunctional compound relative to the diisocyanate compound(s), whereby a hydroxyl-terminated polyurethane prepolymer is formed; and (B) converting the polyurethane prepolymer and one or more isocyanate silane(s) of the formula (I): OCN—R—Si—(R1)m(-OR2)3-m, where m is 0, 1 or 2, each R2 is an alkyl radical having 1 to 4 carbon atoms, each R1 is an alkyl radical having 1 to 4 carbon atoms, and R is a difunctional organic group. Also compounds comprising the silylated polyurethane that can be so produced, and the use thereof as an adhesive and sealant or coating composition.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.