Process for producing a single-crystal component made of a nickel-based superalloy

US8435362B2 · kind B2 · utility

0Cited by
5References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 28, 2011
Grant dateMay 7, 2013
Priority date
Expiry dateAug 2, 2031

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C1/02
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

In a process for producing a large single-crystal component or directionally solidified component made of a nickel-based superalloy, the component is first cast into shape in a known manner to form a microstructure comprising dendrites, and then solution annealing for homogenizing the cast microstructure of the component and two-stage precipitation heat treatment are carried out. In order to avoid chemical inhomogeneities and internal stresses caused thereby, a HIP process with a pressure of higher than 160 MPa is carried out following the solution annealing.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.