Hydrogenated styrenic block copolymers blends with polypropylene
US8445087B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Dec 14, 2009 |
| Grant date | May 21, 2013 |
| Priority date | — |
| Expiry date | May 5, 2030 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31855
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The present invention comprises a molding composition comprising at least about 70% wt. polypropylene or polypropylene random copolymer; up to about 30 wt. % of a block copolymer composition comprising at least one selectively hydrogenated block copolymer which substantially matches the index of refraction of the polypropylene or polypropylene random copolymer, and up to about 0.70% by wt. of a clarifying agent, wherein the weight % of the total blend is 100%. The present invention also may be a molded article produced from the molding composition. A molded article formed from such a composition at a thickness of 0.125 inches will have a haze of less than about 50% and an instrumented impact toughness of at least 100 inch-lbs at −20° C. to −30° C.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.