Patent · US Active

Hot stretch straightening of high strength α/β processed titanium

US8499605B2 · kind B2 · utility

29Cited by
119References
16Claims
0Family size

Assignee

Inventor

Key dates

Filing dateJul 28, 2010
Grant dateAug 6, 2013
Priority date
Expiry dateAug 5, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12299
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for straightening a solution treated and aged (STA) titanium alloy form includes heating an STA titanium alloy form to a straightening temperature of at least 25° F. below the age hardening temperature, and applying an elongation tensile stress for a time sufficient to elongate and straighten the form. The elongation tensile stress is at least 20% of the yield stress and not equal to or greater than the yield stress at the straightening temperature. The straightened form deviates from straight by no greater than 0.125 inch over any 5 foot length or shorter length. The straightened form is cooled while simultaneously applying a cooling tensile stress that balances the thermal cooling stress in the titanium alloy form to thereby maintain a deviation from straight of no greater than 0.125 inch over any 5 foot length or shorter length.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.