Patent · US Active

Fabrication method of ZnO nano-particle and fabrication method of ZnO nano-fluid using thereof

US8512672B2 · kind B2 · utility

4Cited by
1References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 24, 2010
Grant dateAug 20, 2013
Priority date
Expiry dateMay 7, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2982
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

Provided are a method for preparing zinc oxide (ZnO) nanoparticles and a method for preparing ZnO nanofluid using the same. The method for preparing ZnO nanoparticles includes: a) heating deionized water; b) dissolving zinc (Zn) salt in the deionized water to prepare a precursor solution; c) adding solid alkali salt to the precursor solution to prepare a dispersion of ZnO nanoparticles; and d) separating the ZnO nanoparticles by solid-liquid separation and washing them with deionized water. Highly pure, crystalline ZnO nanoparticles with spherical shape and very narrow particle size distribution of 10 to 50 nm can be prepared quickly and at large scale and low cost using inexpensive materials via a stable low-temperature process, without using a dispersant. The associated low-temperature, normal-pressure process produces few harmful materials and may be easily employed for production of ZnO nanoparticles.