Process for catalytic cracking with fine control of the residual coke content on the catalyst after regeneration

US8551326B2 · kind B2 · utility

0Cited by
7References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 15, 2011
Grant dateOct 8, 2013
Priority date
Expiry dateOct 25, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P30/40
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

This invention describes a two-stage regeneration zone that has a regenerated catalyst circuit such as the one that results from the mixing of a partially regenerated catalyst with a residual coke rate of between 0.3 and 0.7% and a totally regenerated catalyst with a coke rate that is less than 0.15%. All things being equal, this double-population regenerated catalyst enables the maximization of the LCO yield.