Tube and heat exchanger using the same, and method of manufacturing tube

US8561682B2 · kind B2 · utility

1Cited by
7References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 5, 2010
Grant dateOct 22, 2013
Priority date
Expiry dateMay 21, 2032

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/49391
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

A tube for a heat exchanger is formed by bending a three-layer clad material of an aluminum alloy to have an overlapped portion. The three-layer clad material is formed by a core material layer containing Mg not smaller than 0.2 wt % after brazing, a brazing material layer on one surface of the core material layer, and a high melting-point material layer on the other surface of the core material layer. The brazing material layer has a thickness not smaller than 25 μm before the brazing, and has a melting point lower than 600° C. The high melting-point material layer has a melting point equal to or higher than 600° C. In addition, the brazing material layer and the high melting-point material layer opposite to each other in the overlapped portion are bonded by the brazing at a temperature not lower than 450° C. for a time within 12 minutes.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.