Patent · US Active

Method of manufacturing and using rod-shaped proppants and anti-flowback additives

US8562900B2 · kind B2 · utility

9Cited by
200References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 17, 2007
Grant dateOct 22, 2013
Priority date
Expiry dateNov 22, 2027

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2235/94
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

A sintered rod-shaped proppant and anti-flowback agent possesses high strength and high conductivity. The sintered rods comprise between about 0.2% by weight and about 4% by weight aluminum titanate. In some embodiments, the sintered rods are made by mixing bauxitic and non-bauxitic sources of alumina that may also contain several so-called impurities (such as TiO2), extruding the mixture, and sintering it. The starting material may optionally be milled to achieve better compacity and crush resistance in the final sintered rod. A fracturing fluid may comprise the sintered rods alone or in combination with a proppant, preferably a proppant of a different shape.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.