Spark plug including high temperature performance electrode

US8575829B2 · kind B2 · utility

1Cited by
5References
21Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 15, 2010
Grant dateNov 5, 2013
Priority date
Expiry dateJan 12, 2031

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/49002
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A spark plug includes at least one electrode having a sparking end. The sparking end is formed of a high temperature performance alloy including chromium in an amount of 10.0 weight percent to 60.0 weight percent, palladium in an amount of 0.5 weight percent to 10.0 weight percent, and a balance substantially of at least one of molybdenum and tungsten. The sparking end presents a spark contact surface, and at a temperature of at least 500° C., such as during use of the spark plug in an internal combustion engine, a layer of chromium oxide (Cr2O3) forms at said spark contact surface. The layer of Cr2O3 protects the bulk of the sparking end from the extreme conditions of the combustion chamber and prevents erosion, corrosion, and balling.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.