Synthesis of LIFEPO4 under hydrothermal conditions
US8586241B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Aug 25, 2009 |
| Grant date | Nov 19, 2013 |
| Priority date | — |
| Expiry date | Aug 1, 2030 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
The present invention relates to a process for the preparation of compounds of general Formula (I) La-bM1bFe1-cM2cPd-eM3eOx (I), wherein Fe has the oxidation state +2 and M1, M2, M3, a, b, c, d, e and x are: M1: Na, K, Rb and/or Cs, M2: Mn, Mg, Al, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, F a: 0.8-1.9, b: 0-0.3, c: 0-0.9, 15 d: 0.8-1.9, e: 0-0.5, x: 1.0-8, depending on the amount and oxidation state of Li, M1, M2, P, M3, wherein compounds of general Formula (I) are neutrally charged, comprising the following steps (A) providing a mixture comprising at least one lithium-comprising compound, at least one iron-comprising compound, in which iron has the oxidation state +3, and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, and at least one reducing agent which is oxidized to at least one compound comprising at least one phosphorous atom in oxidation state +5, and (B) heating the mixture obtained in step (A) at a temperature of 100 to 500° C. and at an autogeneous pressure to reduce Fe to oxidation state +2 and to obtain a compound of general Formula (I).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.