Patent · US Active

Method for reducing carbon dioxide

US8597488B2 · kind B2 · utility

0Cited by
0References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 31, 2012
Grant dateDec 3, 2013
Priority date
Expiry dateMay 31, 2032

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB01J27/24
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

The method for reducing carbon dioxide of the present disclosure includes a step (a) and a step (b) as follows. A step (a) of preparing an electrochemical cell. The electrochemical cell comprises a working electrode, a counter electrode and a vessel. The vessel stores an electrolytic solution. The working electrode contains at least one nitride selected from the group consisting of titanium nitride, zirconium nitride, hafnium nitride, tantalum nitride, molybdenum nitride and iron nitride. The electrolytic solution contains carbon dioxide. The working electrode and the counter electrode are in contact with the electrolytic solution. A step (b) of applying a negative voltage and a positive voltage to the working electrode and the counter electrode, respectively, to reduce the carbon dioxide.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.