Increasing the strength of iridium, rhodium, and alloys thereof
US8613788B2 · kind B2 · utility
0Cited by
6References
1Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jun 28, 2010 |
| Grant date | Dec 24, 2013 |
| Priority date | — |
| Expiry date | Feb 1, 2031 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22F1/14
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The addition of 0.5 to 30 ppm boron and 0.5 to 20 ppm calcium to iridium and the Zr- and Hf-free alloys thereof and rhodium and the Zr- and Hf-free alloys thereof surprisingly increases the creep rupture strength at high temperatures, in particular around 1,800° C.