Use of codoping to modify the scintillation properties of inorganic scintillators doped with trivalent activators

US8617422B2 · kind B2 · utility

54Cited by
4References
15Claims
0Family size

Assignees

Inventors

Key dates

Filing dateSep 28, 2009
Grant dateDec 31, 2013
Priority date
Expiry dateMar 2, 2030

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC30B15/00
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

Crystals with improved scintillation and optical properties are achieved by codoping with a trivalent dopant and a divalent and/or a monovalent dopant. Embodiments include codoping LSO, YSO, GSO crystals and LYSO, LGSO, and LYGSO crystals. Embodiments also include codoped crystals with a controlled monovalent or divalent:trivalent dopant ratio of from about 1:1 for increased light yield to about 4:1 for faster decay time.