Mg alloy and method of production of same

US8636853B2 · kind B2 · utility

0Cited by
1References
7Claims
0Family size

Assignees

Inventors

Key dates

Filing dateMar 26, 2008
Grant dateJan 28, 2014
Priority date
Expiry dateFeb 13, 2029

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/06
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An Mg alloy provided with high strength and high ductility by matching the strength and ductility in tensile deformation and compressive deformation at the same levels is provided. The Mg alloy of the present invention is characterized by having a chemical composition consisting of Y: 0.1 to 1.5 at % and a balance of Mg and unavoidable impurities and having a microstructure with high Y regions with Y concentrations higher than an average Y concentration distributed at nanometer order sizes and intervals. The present invention further provides an Mg alloy characterized by having a chemical composition consisting of Y: more than 0.1 at % and a valance of Mg and unavoidable impurities, having a microstructure with high Y regions with Y concentrations higher than an average Y concentration distributed at nanometer order sizes and intervals and having an average recrystallized grain size within the range satisfying the following formula 1:−0.87c+1.10<log d<1.14c+1.48,  formula 1:where c: Y content (at %) andd: average recrystallized grain size (μm).

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.